White
A film composed of 70-µm calendered, polymeric PVC, which is coated with a pressure-sensitive, extra-reinforced, permanent adhesive. Due to its extra-reinforced adhesive, this product is particularly recommended for application to irregular surfaces, such as bricks, concrete, chipboard, etc. or low-energy surfaces (polyethylene, polypropylene, etc.). Usable for solvent, eco-solvent, latex and UV inkjet printing. They have a glossy surface finish.
Samenstelling & formaat
| Filmtype | polymeric PVC |
| Dikte | 70 µm |
| Kleeflaag | clear |
| Liner | Liner PE |
| Breedte (mm) | 1050,1370 |
| Lengte (m) | 40 |
Verwerking
| Toepassing | ext/int decoration |
| Ondergronden | windows, signage, walls |
| Oppervlakken | textured – low-energy |
| Minimale aanbrengtemperatuur | +10 °C (+50 °F) |
| Gebruiksbereik | -40 °C to +90 °C (-40 °F to +194 °F) |
| Duurzaamheid | long term |
Technische eigenschappen
| Tack | 32 N/25 mm |
| Hechting (20 min) | 28 N/25 mm |
| Hechting (24 h) | 31 N/25 mm |
| Afpelkracht liner | 0.1 N/25 mm |
| Treksterkte | min. 35 N/25 mm |
| Rek bij breuk | min. 100 % |
| Krimp (168 h / 70 °C) | < 1 mm |
Toepassing & onderhoud
Due to the wide variety of existing substrates, the application of film to an unsuitable and/or not adequately prepared surface or coating may result in media lifting from the substrate or damage to the substrate when the film is removed. The application and removal of the film are at the judgement and risk of the installer. HEXIS will not, under any circumstances, be liable for any damages or deteriorations caused by the installation or removal of a vinyl film.
- For application to irregular surfaces, the substrate must be cleared of all traces of dust to ensure optimum adhesion of the film.
- In the case of painted substrates, self-adhesive media must only be applied to undamaged original paintwork. If the paintwork is not original and/or damaged, the application and the removal are at the judgement and risk of the installer.
If necessary, refurbish the substrate or existing laminate before applying the vinyl. A drying time of 7-10 days may be needed before proceeding with the film application. The degassing of an undried paint can lead to lifting, bubbles and tearing of the film.
Aanbevelingen
- Optimal drying time for the inks before laminating or further processing is 24 hours minimum.
- The surface finish of the prints may be modified/improved/protected by applying the appropriate laminate: PC500 or V750. For UV prints, use the protective VCR750 laminate.
Duurzaamheid in detail
- Vertical outdoor exposure:
Blank unprinted: 8 years.
Printed and laminated:
- PC500: 5 years.
- V750: 4 years.
- VCR750: 3 years.
Printed: 2 years
- Vertical outdoor exposure on irregular surfaces (brick, concrete, chipboard, etc.): Printed and laminated with PC500, V750 or VCR750: 3 to 6 months depending on exposure and climate conditions.