White
Film composed of 70-µm calendered, polymeric PVC, which is coated with a super-reinforced, pressure-sensitive, grey acrylic adhesive. Particularly recommended for application to walls (e.g. Placoplatre® BA13 plasterboard, smooth or slightly textured walls) or low-energy surfaces (polyethylene, polypropylene, etc.). Usable for solvent, eco-solvent, latex and UV inkjet printing. It has a glossy surface finish.
Samenstelling & formaat
| Filmtype | polymeric PVC |
| Dikte | 70 µm |
| Kleeflaag | grey |
| Liner | Liner PE |
| Breedte (mm) | 1050,1370 |
| Lengte (m) | 45 |
Verwerking
| Toepassing | ext/int decoration |
| Ondergronden | windows, signage, walls |
| Oppervlakken | textured – low-energy |
| Minimale aanbrengtemperatuur | +10 °C (+50 °F) |
| Gebruiksbereik | -40 °C to +90 °C (-40 °F to +194 °F) |
| Duurzaamheid | long term |
Technische eigenschappen
| Tack | 24 N/25 mm |
| Hechting (20 min) | 25 N/25 mm |
| Hechting (24 h) | 29 N/25 mm |
| Afpelkracht liner | 0.1 N/25 mm |
| Treksterkte | min. 20 N/25 mm |
| Krimp (168 h / 70 °C) | < 0.8 mm |
Toepassing & onderhoud
Due to the wide variety of existing substrates, the application of film to an unsuitable and/or not adequately prepared surface or coating may result in media lifting from the substrate or damage to the substrate when the film is removed. The application and removal of the film are at the judgement and risk of the installer. HEXIS will not, under any circumstances, be liable for any damages or deteriorations caused by the installation or removal of a vinyl film.
- Very good adhesion to glass, steel, aluminium, PVC, melamine, smooth or slightly textured surfaces (e.g. Placoplatre® BA13 plasterboard, etc.), except for granular, chalky, damaged substrates (cracks, holes, humidity or condensation spots, excess of texture, etc.) or substrates coated with acrylic paints, etc.
- Due to the wide variety of existing substrates, a preliminary tear-off test must be carried out on a small inconspicuous surface of the substrate using a small piece of film.
If necessary, refurbish the substrate or existing coating before applying the vinyl.
- Carry out a degassing test on freshly painted surfaces before applying any film.
A drying time of 7-10 days may be necessary before proceeding with the vinyl application. The degassing of a non-dried paint can lead to lifting, bubbles and tearing of the film.
Aanbevelingen
- Optimal drying time for the inks before laminating or further processing is 24 hours minimum.
- The surface finish of the prints may be modified/improved/protected by applying the appropriate laminate: V750 or PC500. For UV prints, use the protective VCR750 laminate.
Duurzaamheid in detail
- Vertical outdoor exposure:
Blank: 8 years.
Printed and laminated:
- PC500: 5 years.
- V750: 4 years.
- VCR750: 3 years.
Printed: 2 years