Transparent
Film composed of an 80-µm calendered, monomeric PVC, which is coated with a pressure-sensitive acrylic adhesive. Matt surface finish for cold lamination, mainly for use as a mechanical protection. Particularly suitable for laminating UV inkjet printing.
Samenstelling & formaat
| Filmtype | Monomeric PVC |
| Dikte | 80 µm |
| Kleeflaag | clear |
| Liner | Liner kraft |
| Breedte (mm) | 1370 |
| Lengte (m) | 50 |
Verwerking
| Toepassing | promotional decoration |
| Ondergronden | windows, signage, walls |
| Oppervlakken | flat |
| Minimale aanbrengtemperatuur | +10 °C to +35 °C (+50 °F to +95 °F) |
| Gebruiksbereik | -30 °C to +60 °C (-22 °F to +140 °F) |
| Duurzaamheid | short term |
Technische eigenschappen
| Tack | 22 N/25 mm |
| Hechting (20 min) | 19 N/25 mm |
| Hechting (24 h) | 21 N/25 mm |
| Afpelkracht liner | 0.2 N/25 mm |
| Treksterkte | min. 30 N/25 mm |
| Krimp (168 h / 70 °C) | < 1.2 mm |
Toepassing & onderhoud
- Particularly suitable for cold laminating UV inkjet prints.
Although the ink is solid immediately after printing, the polymerisation and reticulation time of the inks is 24 hours (variable depending upon the printer used and the quantity of ink applied). Please comply with this minimum waiting time before laminating the UV inkjet-printed film.
- Resistance against mechanical stress.
- Using this protective film also enables you to modify the products’s visual aspect by providing it with a matt surface finish.
- Depending on the type of surface to be protected: when applied to paintworks or "non dry" inkjet prints, the VCR650M laminate may show signs of shrinkage. To avoid such alterations or for medium-term applications, we strongly recommend the use of our VCR750 laminate.
- In the case of an already painted substrate, apply to undamaged original paintwork only. If the paintwork is not original and/or damaged, the application and the removal are at the judgement and risk of the installer.
Duurzaamheid in detail
- Up to 1.5 years only for the laminate but not for the graphics.
The durability of the laminated print depends on the printing technology used and the inks used. Consult the ink manufacturer.